Polymer Property : Thermal Conductivity = 296 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 42.7 W/m-K

@Temperature 100 °C
296 BTU-in/hr-ft²-°F

@Temperature 212 °F
Latrobe LSSâ„¢ 4140 Alloy Steel (AISI 4140)
TLS 4140 and 4142HT are versatile, alloy steels which are used in variety of tooling and other industrial applications. TLS 4140 is the classic AISI 4140 alloy steel which is sold in the annealed co..