Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 29.3 W/m-K @Temperature 400 °C |
203 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
International Mold Steel DH21 Die Cast & Forging Steel DH21 is for aluminum die cast dies.Information provided by International Mold Steel |
|||
Thermal Conductivity | 29.3 W/m-K @Temperature 600 °C |
203 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
International Mold Steel DH21 Die Cast & Forging Steel DH21 is for aluminum die cast dies.Information provided by International Mold Steel |
|||
Thermal Conductivity | 29.3 W/m-K @Temperature 704 °C |
203 BTU-in/hr-ft²-°F @Temperature 1300 °F |
|
Schmolz + Bickenbach Thermodur® 2365 EFS Extra Fine Structure - Hot Work Die Steel Description: Thermodur® 2365 is an Extra Fine Structure (EFS) hot work tool steel developed for good high temperature strength and tempering resistance and Supplied in the annealed conditionChara.. |