Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 2.20 - 4.20 W/m-K @Temperature 1400 °C |
15.3 - 29.1 BTU-in/hr-ft²-°F @Temperature 2550 °F |
|
Gouda Vuurvast VIBRON 160 K 50 Dense Vibrating Refractory Castable Description: Vibron 160 K 50 is a low cement castable based on silicon carbide and characterized by a very good thermal conductivity, high abrasion resistance and a good oxidation resistance up to 1.. |