Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 29.0 W/m-K @Temperature 1100 °C |
201 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Special Metals INCOLOY® alloy 864 INCOLOY® alloy 8684 (UNS S35135) was specifically developed for automotive exhaust system flexible couplings, EGR tubes, manifolds and tailpipes. It exhibits excellent fatigue resistance, therma.. |
|||
Thermal Conductivity | 29.0 W/m-K @Temperature 100 °C |
201 BTU-in/hr-ft²-°F @Temperature 212 °F |
Hardened and tempered |
Bohler-Uddeholm BÖHLER W303 ISODISC® Hot Work Tool Steel Description: Hot work tool steel featuring excellent hot tensile properties, high retention of hardness, good toughness and resistance to heat checking, admits water cooling. BOHLER W303 is also ava.. |
|||
Thermal Conductivity | 29.0 W/m-K @Temperature 20.0 °C |
201 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
hardened to 310 HB |
Bohler-Uddeholm P20 PREMIUM MODIFIED Pre-hardened Mold Steel Cr-Mo alloyed steelP20 Modified offers the following benefits:No hardening risksNo hardening costsTime saving, e.g. no waiting for heat treatmentLower tool cost (e.g. no distortion to rectify)Modifi.. |
|||
Thermal Conductivity | 29.0 W/m-K @Temperature 399 °C |
201 BTU-in/hr-ft²-°F @Temperature 750 °F |
hardness of 45 HRC |
Bohler-Uddeholm UDDEHOLM ORVAR® SUPERIOR (Premium AISI H13) Hot Work Tool Steel Chromium-molybdenum-vanadium alloyed steelA premium Cr-Mo-V-alloyed hot work die steel with good resistance to thermal fatigue. The steel is produced by a special melting and refining technique in o.. |
|||
Thermal Conductivity | 29.0 W/m-K @Temperature 399 °C |
201 BTU-in/hr-ft²-°F @Temperature 750 °F |
hardness of 45 HRC |
Bohler-Uddeholm UDDEHOLM ORVAR® SUPREME (Premium AISI H13) Hot Work Tool Steel Chromium-molybdenum-vanadium alloyed steelA premium Cr-Mo-V-alloyed hot work die steel with good resistance to thermal fatigue. The steel is produced by a special melting and refining technique in o.. |
|||
Thermal Conductivity | 29.0 W/m-K @Temperature 150 °C |
201 BTU-in/hr-ft²-°F @Temperature 302 °F |
Quenched and Tempered |
Schmolz + Bickenbach Cryodur® 2767 Cold Work Die Steel Description: High hardenability and toughness, highly suitable for polishing, texturing and EDM machining. We recommend the use of Cryodur® 2767 (ERS) for extreme demandsApplications: Cutlery dies,.. |