Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 40.3 W/m-K @Temperature 204 °C |
280 BTU-in/hr-ft²-°F @Temperature 400 °F |
|
Schmolz + Bickenbach Cryodur® 2312 (Brake Die) Cold Work Die Steel Description: Cryodur® 2312 is a pre-hardened single melt Extra Fine Structure (EFS) plastic mold steel and Re-sulphurized to improve machinabilityCharacteristics: Excellent machinability compared t.. |
|||
Thermal Conductivity | 40.3 W/m-K @Temperature 204 °C |
280 BTU-in/hr-ft²-°F @Temperature 400 °F |
|
Schmolz + Bickenbach Formadur® 2312 (Ultra Holder) Plastic Mold Steel Description: Formadur® 2312 is a pre-hardened single melt Extra Fine Structure (EFS) plastic mold steel and Re-sulphurized to improve machinabilityCharacteristics: Excellent machinability compared .. |