Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 39.9 W/m-K @Temperature 500 °C |
277 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
American Utility Metals Cromgard® Stainless Steel Cromgard is a low cost stainless steel, which is able to provide benefits of good weldability and formability, making it capable of fabrication by conventional techniques. It provides the benefits o.. |