Thermal Properties Metric English Comments
Thermal Conductivity 39.5 W/m-K

@Temperature 350 °C
274 BTU-in/hr-ft²-°F

@Temperature 662 °F
Annealed
Schmolz + Bickenbach Thermodur® 2999 Hot Work Die Steel
Description: Maximum high-temperature strength, good high-temperature wear resistance, excellent thermal shock resistance and thermal conductivity across the entire range of service temperatures App..
Thermal Conductivity 39.5 W/m-K

@Temperature 700.0 °C
274 BTU-in/hr-ft²-°F

@Temperature 1292 °F
Annealed
Schmolz + Bickenbach Thermodur® 2999 Hot Work Die Steel
Description: Maximum high-temperature strength, good high-temperature wear resistance, excellent thermal shock resistance and thermal conductivity across the entire range of service temperatures App..