Thermal Properties Metric English Comments
Thermal Conductivity 27.9 W/m-K

@Temperature 100 °C
194 BTU-in/hr-ft²-°F

@Temperature 212 °F
QuesTek® Innovations Ferrium® M54™ Ultrahigh-strength Steel for Structural Applications
Description: Ferrium® M54™ is an ultra high-strength steel for structural applications. Ferrium® M54™ was designed to provide mechanical properties equal to, or better than ultrahigh-strength st..
Thermal Conductivity 27.9 W/m-K

@Temperature 300 °C
194 BTU-in/hr-ft²-°F

@Temperature 572 °F
International Mold Steel Daido DRM2 Matrix High-Speed Steel
This matrix type high speed tool steel is available for warm and cold forging tools where critical performance is required. DRM2 prolongs service life due to its higher hardness and toughness than t..
Thermal Conductivity 27.9 W/m-K

@Temperature 760 °C
194 BTU-in/hr-ft²-°F

@Temperature 1400 °F
Latrobe LSSâ„¢ H12 Hot Work Tool Steel (ASTM H12)
TLS H12 hot work tool steel is a 5% chromium, general-purpose hot work steel that is characterized by excellent impact toughness. It contains less vanadium than the widely-used H13 hot work tool ste..
Thermal Conductivity 27.9 W/m-K

@Temperature 300 °C
194 BTU-in/hr-ft²-°F

@Temperature 572 °F
International Mold Steel DHA-World Die Cast & Forging Steel
DHA-World is a high hardenability and high tough general use hot work die steel.Information provided by International Mold Steel