Polymer Property : Thermal Conductivity = 25.2 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 25.2 W/m-K

@Temperature 100 °C
175 BTU-in/hr-ft²-°F

@Temperature 212 °F
International Mold Steel DHA-World Die Cast & Forging Steel
DHA-World is a high hardenability and high tough general use hot work die steel.Information provided by International Mold Steel
Thermal Conductivity 25.2 W/m-K

@Temperature 816 °C
175 BTU-in/hr-ft²-°F

@Temperature 1500 °F
Crucible Steel XM-19 Stainless Steel
Crucible XM-19 Stainless is a nitrogen strengthened, low carbon, austenitic, stainless steel that provides good corrosion resistance in combination with high strength. The alloy has better corrosio..
Thermal Conductivity 25.2 W/m-K

@Temperature 46.0 °C
175 BTU-in/hr-ft²-°F

@Temperature 115 °F
perpendicular to c-axis
Mateck Sapphire (Al2O3)
Optical crystals