Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 22.9 W/m-K @Temperature 20.0 °C |
159 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
EDRO #8 Premium 420 Stainless Mold Steel EDRO #8™ is a chromium-alloyed stainless tool steel with the following properties: excellent corrosion resistance, superior polishability, good wear resistance, good machinability, and stability in.. |