Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 22.7 W/m-K @Temperature 800 °C |
158 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes Waspaloy™ alloy, sheet Age-hardenable superalloy with very good strength at temperatures up 980°C (1800°F), can be cold-formed in the annealed condition, may also be hot formed at 1040°C (1900°F) and above, go.. |
|||
Thermal Conductivity | 22.7 W/m-K @Temperature 800 °C |
158 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes X-750 Nickel Alloy Sheet and Strip (AMS 5598, UNS N07750) Haynes X-750 (UNS No. N07750) alloy is an age-hardenable, nickel-base superalloy with very good strength at temperatures up to about 1600°F (870°C). It is widely used as a wrought material for.. |
|||
Thermal Conductivity | 22.7 W/m-K @Temperature 600 °C |
158 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Haynes 75 Nickel Alloy Sheet, Annealed at 1925°F (1050°C) Haynes alloy 75 is a solution-strengthened nickel-chromium alloy with moderate strength to 1200°F (650°C). It is principally used in low stress elevated temperature applications requiring reas.. |
|||
Thermal Conductivity | 22.7 W/m-K @Temperature 200 °C |
158 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
QuesTek® Innovations Ferrium® S53® Corrosion Resistant High Strength Steel for Aerospace Structural Applications Description: Ferrium® S53® is a corrosion resistant ultra high-strength steel for structural aerospace applications. Ferrium® S53® was designed to provide mechanical properties equal to, or bett.. |