Polymer Property : Thermal Conductivity = 22.2 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 3.20 W/m-K

@Temperature 650 °C
22.2 BTU-in/hr-ft²-°F

@Temperature 1200 °F
Gouda Vuurvast AC 90-8 Dense Refractory Brick
Description: Excellent resistance against alkali- and metal slags. The 8% chromium-oxide addition gives good volume stability at very high temperatures. Applications: chemical incinerators, combusti..
Thermal Conductivity 3.20 W/m-K

@Temperature 650 °C
22.2 BTU-in/hr-ft²-°F

@Temperature 1200 °F
Gouda Vuurvast AK 98 Dense Refractory Brick
Description: This high alumina brick finds wide application in chemical reactors. The firing temperature of these bricks is very high, which results in an improved thermal shock resistance and bette..
Thermal Conductivity 3.20 W/m-K

@Temperature 1100 °C
22.2 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Gouda Vuurvast AK 98 Dense Refractory Brick
Description: This high alumina brick finds wide application in chemical reactors. The firing temperature of these bricks is very high, which results in an improved thermal shock resistance and bette..