Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 216 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 31.1 W/m-K

@Temperature 427 °C
216 BTU-in/hr-ft²-°F

@Temperature 800 °F
Schmolz + Bickenbach P-20 High Hard Plastic Mold Steel
Description: P-20 High Hard is an improved pre-hardened mold steel that has been specially designed for large plastic molds; Material is forged on a 5000 ton press assuring maximum deformation durin..
Thermal Conductivity 31.1 W/m-K

@Temperature 427 °C
216 BTU-in/hr-ft²-°F

@Temperature 800 °F
Schmolz + Bickenbach P-20 Modified Plastic Mold Steel
Description: P-20 Modified is an improved pre-hardened mold steel that has been specially designed for large plastic molds; The material is forged on a 5000 ton press assuring maximum deformation du..
Thermal Conductivity 31.1 W/m-K

@Temperature 399 °C
216 BTU-in/hr-ft²-°F

@Temperature 750 °F
EDRO #3 Prehardened Mold Quality P20 Alloy Steel
EDRO #3™ is a vacuum-degassed, ladle refined, Cr-Ni-Mo- alloyed steel which is supplied in the hardened and tempered condition. EDRO #3™ is manufactured to consistently high quality standards with..
Thermal Conductivity 31.1 W/m-K

@Temperature 600 °C
216 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Bohler-Uddeholm BÖHLER M268 VMR® Plastic Mold Steel
Description: HBÖHLER M268 VMR is a hardened and tempered plastic mould steel with excellent cleanliness for best polishability. The hardness is constant over the entire cross-section of the steel b..
Thermal Conductivity 31.1 W/m-K

@Temperature 300 °C
216 BTU-in/hr-ft²-°F

@Temperature 572 °F
Hardened and tempered
Bohler-Uddeholm BÖHLER W303 ISODISC® Hot Work Tool Steel
Description: Hot work tool steel featuring excellent hot tensile properties, high retention of hardness, good toughness and resistance to heat checking, admits water cooling. BOHLER W303 is also ava..
Thermal Conductivity 31.1 W/m-K

@Temperature 400 °C
216 BTU-in/hr-ft²-°F

@Temperature 752 °F
Hardened and tempered
Bohler-Uddeholm BÖHLER W303 ISODISC® Hot Work Tool Steel
Description: Hot work tool steel featuring excellent hot tensile properties, high retention of hardness, good toughness and resistance to heat checking, admits water cooling. BOHLER W303 is also ava..
Thermal Conductivity 31.1 W/m-K

@Temperature 399 °C
216 BTU-in/hr-ft²-°F

@Temperature 750 °F
Schmolz + Bickenbach Holder Block Plastic Mold Steel
Description: Holder Block is a modified AISI-4130 material with higher chromium and molybdenum content specifically designed holder steel for molds and dies and The material is forged on a 5000 ton..