Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 30.8 W/m-K @Temperature 704 °C |
214 BTU-in/hr-ft²-°F @Temperature 1300 °F |
|
Schmolz + Bickenbach Cryodur® 2510 (O-1) Cold Work Die Steel Description: Cyrodur ® 2510 is a single melt Extra Fine Structure (EFS) material; and Supplied in the soft annealed conditionCharacteristics: Excellent dimensional stability during heat treatment; .. |