Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 30.1 W/m-K @Temperature 1000 °C |
209 BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
Haynes 75 Nickel Alloy Sheet, Annealed at 1925°F (1050°C) Haynes alloy 75 is a solution-strengthened nickel-chromium alloy with moderate strength to 1200°F (650°C). It is principally used in low stress elevated temperature applications requiring reas.. |
|||
Thermal Conductivity | 30.1 W/m-K @Temperature 204 °C |
209 BTU-in/hr-ft²-°F @Temperature 400 °F |
|
Schmolz + Bickenbach P-20 High Hard Plastic Mold Steel Description: P-20 High Hard is an improved pre-hardened mold steel that has been specially designed for large plastic molds; Material is forged on a 5000 ton press assuring maximum deformation durin.. |
|||
Thermal Conductivity | 30.1 W/m-K @Temperature 204 °C |
209 BTU-in/hr-ft²-°F @Temperature 400 °F |
|
Schmolz + Bickenbach P-20 Modified Plastic Mold Steel Description: P-20 Modified is an improved pre-hardened mold steel that has been specially designed for large plastic molds; The material is forged on a 5000 ton press assuring maximum deformation du.. |
|||
Thermal Conductivity | 30.1 W/m-K @Temperature 400 °C |
209 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Bohler-Uddeholm BÖHLER W403 VMR® Hot Work Tool Steel W403 VMR is a modified hot work alloy with an excellent combination of hot tensile properties and toughness. The balanced properties of this grade are not only due to chemistry modification, but to .. |
|||
Thermal Conductivity | 30.1 W/m-K @Temperature 204 °C |
209 BTU-in/hr-ft²-°F @Temperature 400 °F |
|
Schmolz + Bickenbach Holder Block Plastic Mold Steel Description: Holder Block is a modified AISI-4130 material with higher chromium and molybdenum content specifically designed holder steel for molds and dies and The material is forged on a 5000 ton.. |