Polymer Property : Thermal Conductivity = 2.71 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.290 - 0.390 W/m-K

@Temperature 600 °C
2.01 - 2.71 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast GI 26 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Thermal Conductivity 0.290 - 0.390 W/m-K

@Temperature 1200 °C
2.01 - 2.71 BTU-in/hr-ft²-°F

@Temperature 2190 °F
Gouda Vuurvast GOLITE 120 Refractory Insulating Castable
Description: Golite 120 is composed of light weight aggregates, alumina cement and special additions to be sure of a high strength and a low firing shrinkage.Remarks: These values apply to cast prod..