Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 26.78 W/m-K @Temperature 1200 °C |
185.9 BTU-in/hr-ft²-°F @Temperature 2190 °F |
|
Latrobe LSSâ„¢ H11 Hot Work Tool Steel (ASTM H11) TLS H11 hot work tool steel is a 5% chromium hot work steel that is characterized by excellent impact toughness. It contains less vanadium than the widely-used H13 hot work tool steel. This provides.. |