Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 24.5 W/m-K @Temperature 900 °C |
170 BTU-in/hr-ft²-°F @Temperature 1650 °F |
|
Haynes Waspaloy™ alloy, sheet Age-hardenable superalloy with very good strength at temperatures up 980°C (1800°F), can be cold-formed in the annealed condition, may also be hot formed at 1040°C (1900°F) and above, go.. |
|||
Thermal Conductivity | 24.5 - 25.5 W/m-K @Temperature 400 °C |
170 - 177 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Bohler-Uddeholm UDDEHOLM Vancron 40 nitrided powder tool steel Description: Uddeholm Vancron 40 is a nitrided powder tool steel, which means that a “surface coating” is already integrated into the finished tooling material. The result is a tool surface with v.. |