Polymer Property : Thermal Conductivity = 165 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 23.8 W/m-K

@Temperature 900 °C
165 BTU-in/hr-ft²-°F

@Temperature 1650 °F
Special Metals INCONEL® alloy 740 Precipitation-Hardenable Ni-Cr-Co Superalloy
INCONEL® alloy 740 is a nickel-chromium-cobalt alloy developed by Special Metals Corporation. The alloy is age hardenable by the precipitation of a gamma prime second phase. Potential applicati..
Thermal Conductivity 23.8 W/m-K

@Temperature 816 °C
165 BTU-in/hr-ft²-°F

@Temperature 1500 °F
ATI Allvac® 718Plus™ Nickel Superalloy
Allvac 718Plus alloy (UNS N07818) is a precipitation hardened nickel-base material that exhibits high temperature tensile strength and stress rupture performance. This alloy is designed to have the..
Thermal Conductivity 23.8 W/m-K

@Temperature 343 °C
165 BTU-in/hr-ft²-°F

@Temperature 650 °F
Schmolz + Bickenbach CorroPlast® Plastic Mold Steel
Description: CorroPlast® is a pre-hardened, free-machining 400 series stainless steel, specifically developed for mold bases for processing plastic; and Supplied in the pre-hardened condition with ..