Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 2.44 W/m-K @Temperature 200 °C |
16.9 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Crucible Steel KAPSTAR® Mold Steel Kapstar is a high hard, precipitation hardening mold steel suitable for production of machined or EDM’d plastic mold, rubber mold, and zinc die casting die components. Kapstar is supplied at about .. |