Thermal Properties Metric English Comments
Thermal Conductivity 22.5 W/m-K

@Temperature <=20.0 °C
156 BTU-in/hr-ft²-°F

@Temperature <=68.0 °F
CLAL-MSX ARCAP Anticorrosion AP4 H13 3/4 hard, Drawn Copper Alloy
Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc..
Thermal Conductivity 22.5 W/m-K

@Temperature <=20.0 °C
156 BTU-in/hr-ft²-°F

@Temperature <=68.0 °F
CLAL-MSX ARCAP Anticorrosion AP4 H14 4/4 hard, Drawn Copper Alloy
Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc..
Thermal Conductivity 22.5 W/m-K

@Temperature <=20.0 °C
156 BTU-in/hr-ft²-°F

@Temperature <=68.0 °F
CLAL-MSX ARCAP Anticorrosion AP4 H15 Spring, Drawn Copper Alloy
Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc..
Thermal Conductivity 22.5 W/m-K

@Temperature <=20.0 °C
156 BTU-in/hr-ft²-°F

@Temperature <=68.0 °F
CLAL-MSX ARCAP Anticorrosion AP4 H15 Spring, Rolled Copper Alloy
Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc..
Thermal Conductivity 22.5 W/m-K

@Temperature <=20.0 °C
156 BTU-in/hr-ft²-°F

@Temperature <=68.0 °F
CLAL-MSX ARCAP Anticorrosion AP4 0 Annealed, Drawn Copper Alloy
Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc..
Thermal Conductivity 22.5 W/m-K

@Temperature <=20.0 °C
156 BTU-in/hr-ft²-°F

@Temperature <=68.0 °F
CLAL-MSX ARCAP Anticorrosion AP4 0 Annealed, Rolled Copper Alloy
Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc..
Thermal Conductivity 22.5 W/m-K

@Temperature <=20.0 °C
156 BTU-in/hr-ft²-°F

@Temperature <=68.0 °F
CLAL-MSX ARCAP Anticorrosion AP4 H11 1/4 hard, Drawn Copper Alloy
Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc..
Thermal Conductivity 22.5 W/m-K

@Temperature <=20.0 °C
156 BTU-in/hr-ft²-°F

@Temperature <=68.0 °F
CLAL-MSX ARCAP Anticorrosion AP4 H11 1/4 hard, Rolled Copper Alloy
Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc..
Thermal Conductivity 22.5 W/m-K

@Temperature <=20.0 °C
156 BTU-in/hr-ft²-°F

@Temperature <=68.0 °F
CLAL-MSX ARCAP Anticorrosion AP4 H12 1/2 hard, Drawn Copper Alloy
Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc..
Thermal Conductivity 22.5 W/m-K

@Temperature <=20.0 °C
156 BTU-in/hr-ft²-°F

@Temperature <=68.0 °F
CLAL-MSX ARCAP Anticorrosion AP4 H12 1/2 hard, Rolled Copper Alloy
Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc..
Thermal Conductivity 22.5 W/m-K

@Temperature 93.3 °C
156 BTU-in/hr-ft²-°F

@Temperature 200 °F
Schmolz + Bickenbach Formadur® 2083 Superclean Plastic Mold Steel
Description: Formadur 2083 Superclean is an electro slag remelted (ESR) martensitic stainless steel developed for corrosion resistant applications and Supplied in the annealed conditionCharacteristi..
Thermal Conductivity 22.5 W/m-K

@Temperature 149 °C
156 BTU-in/hr-ft²-°F

@Temperature 300 °F
Schmolz + Bickenbach CorroPlast® Plastic Mold Steel
Description: CorroPlast® is a pre-hardened, free-machining 400 series stainless steel, specifically developed for mold bases for processing plastic; and Supplied in the pre-hardened condition with ..