Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 21.8 W/m-K @Temperature 21.1 °C |
151 BTU-in/hr-ft²-°F @Temperature 70.0 °F |
|
Schmolz + Bickenbach CorroPlast® Plastic Mold Steel Description: CorroPlast® is a pre-hardened, free-machining 400 series stainless steel, specifically developed for mold bases for processing plastic; and Supplied in the pre-hardened condition with .. |