Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 146.8 W/m-K @Temperature 25.0 °C |
1019 BTU-in/hr-ft²-°F @Temperature 77.0 °F |
|
Osprey Metals CE17M Al-Si Controlled Expansion Alloy Al-27%Si+ controlled expansion alloy manufactured and patented by Osprey Metals Ltd.Information provided to MatWeb by Osprey Metals. |