Thermal Properties Metric English Comments
Thermal Conductivity 20.5 W/m-K

@Temperature 500 °C
142 BTU-in/hr-ft²-°F

@Temperature 932 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) All Weld Cruciform
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Thermal Conductivity 20.5 W/m-K

@Temperature 500 °C
142 BTU-in/hr-ft²-°F

@Temperature 932 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Thermal Conductivity 20.5 W/m-K

@Temperature 500 °C
142 BTU-in/hr-ft²-°F

@Temperature 932 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) Sheet
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Thermal Conductivity 20.5 W/m-K

@Temperature 500 °C
142 BTU-in/hr-ft²-°F

@Temperature 932 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate and Bar, Hot-rolled, Solution Annealed
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Thermal Conductivity 20.5 W/m-K

@Temperature 500 °C
142 BTU-in/hr-ft²-°F

@Temperature 932 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Sheet, Cold-rolled, Solution Annealed
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Thermal Conductivity 20.5 W/m-K

@Temperature 500 °C
142 BTU-in/hr-ft²-°F

@Temperature 932 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Sheet, Cold-rolled, Solution Annealed, Age-hardened
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Thermal Conductivity 20.5 W/m-K

@Temperature 500 °C
142 BTU-in/hr-ft²-°F

@Temperature 932 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Thermal Conductivity 20.5 W/m-K

@Temperature 600 °C
142 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Haynes Hastelloy® C-4 alloy, all-weld metal, as welded, GTAW
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) rang..
Thermal Conductivity 20.5 W/m-K

@Temperature 600 °C
142 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Haynes Hastelloy® C-4 alloy, welded plate 12.7 mm (1/2 in.) thick, aged 1000 hours at 649°C (1200°F)
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) rang..
Thermal Conductivity 20.5 W/m-K

@Temperature 700.0 °C
142 BTU-in/hr-ft²-°F

@Temperature 1292 °F
AK Steel 13-4 SR® Ferritic Stainless Steel
AK Steel 13-4 SR Stainless Steel is a ductile weldable ferritic with 13% Cr and 3.75% Al. The high aluminum content results in a base alloy with high electrical resistivity. It is intended for use w..
Thermal Conductivity 20.5 W/m-K

@Temperature 20.0 °C
142 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Assab Steels ASSAB XW-5 Cold Work Steel
ASSAB XW-5 is a high-carbon, high chromium tool steel alloyed with tungsten, characterized by:High wear resistanceHigh compressive strengthHigh surface hardness after hardeningGood through-hardening..
Thermal Conductivity 20.5 W/m-K

@Temperature 500 °C
142 BTU-in/hr-ft²-°F

@Temperature 932 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate and Bar, Hot-rolled, Solution Annealed, Age-hardened
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately doubl..
Thermal Conductivity 20.5 W/m-K

@Temperature 500 °C
142 BTU-in/hr-ft²-°F

@Temperature 932 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately doubl..
Thermal Conductivity 20.5 W/m-K

@Temperature 600 °C
142 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Haynes Hastelloy® C-4 alloy, welded plate 12.7 mm (1/2 in.) thick, aged 10 hours at 649°C (1200°F)
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T..
Thermal Conductivity 20.5 W/m-K

@Temperature 600 °C
142 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Haynes Hastelloy® C-4 alloy, welded plate 12.7 mm (1/2 in.) thick, GTAW
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T..
Thermal Conductivity 20.5 W/m-K

@Temperature 343 °C
142 BTU-in/hr-ft²-°F

@Temperature 650 °F
Schmolz + Bickenbach Cryodur® 2379 (D-2) Cold Work Die Steel
Description: Cryodur® 2379 is a high carbon, high chromium tool steel developed for high wear applications and Supplied in the annealed conditionCharacteristics: Excellent abrasive wear resistance;..