Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 20.2 W/m-K @Temperature 100 °C |
140 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
QuesTek® Innovations Ferrium® S53® Corrosion Resistant High Strength Steel for Aerospace Structural Applications Description: Ferrium® S53® is a corrosion resistant ultra high-strength steel for structural aerospace applications. Ferrium® S53® was designed to provide mechanical properties equal to, or bett.. |