Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 19.0 W/m-K @Temperature 500 °C |
132 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2025°F (1107°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Thermal Conductivity | 19.0 W/m-K @Temperature 500 °C |
132 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Thermal Conductivity | 19.0 W/m-K @Temperature 500 °C |
132 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Thermal Conductivity | 19.0 W/m-K @Temperature 400 °C |
132 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Assab Steels VANADIS 10 Cold Work Steel VANADIS 4 is a chromium-molybdenum-vanadium alloyed steel which is characterized by:Extremely high abrasive wear resistanceHigh compressive strengthVery good through-hardening propertiesGood toughne.. |
|||
Thermal Conductivity | 19.0 W/m-K @Temperature 500 °C |
132 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is.. |