Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 18.9 W/m-K @Temperature 27.0 °C |
131 BTU-in/hr-ft²-°F @Temperature 80.6 °F |
|
Latrobe LSSâ„¢ H12 Hot Work Tool Steel (ASTM H12) TLS H12 hot work tool steel is a 5% chromium, general-purpose hot work steel that is characterized by excellent impact toughness. It contains less vanadium than the widely-used H13 hot work tool ste.. |