Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.82 - 1.92 W/m-K @Temperature 100 °C |
12.6 - 13.3 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast VIBRON 150 G RAPID Dense Vibrating Refractory Castable Description: Vibron 150 G Rapid is a low cement castable based on sintered South-American bauxite. Because of special additives this material is suited for direct contact with liquid aluminum and al.. |
|||
Thermal Conductivity | 1.82 - 1.92 W/m-K @Temperature 600 °C |
12.6 - 13.3 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast VIBRON 150 G RAPID Dense Vibrating Refractory Castable Description: Vibron 150 G Rapid is a low cement castable based on sintered South-American bauxite. Because of special additives this material is suited for direct contact with liquid aluminum and al.. |