Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 12.0 W/m-K @Temperature 100 °C |
83.3 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2025°F (1107°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Thermal Conductivity | 12.0 W/m-K @Temperature 100 °C |
83.3 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Thermal Conductivity | 12.0 W/m-K @Temperature 100 °C |
83.3 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Thermal Conductivity | 12.0 W/m-K @Temperature 100 °C |
83.3 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2075°F (1135°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Thermal Conductivity | 12.0 W/m-K @Temperature 600.0 °C |
83.2 BTU-in/hr-ft²-°F @Temperature 1112 °F |
|
Stellar Canada CERAMITE® CSA Wear Resistant Castable Ceramite is a family of wear resistant castables with a unique combination of high wear resistance, thermal resistance and mechanical strength. Ceramite is produced and supplied to end users world w.. |
|||
Thermal Conductivity | 12.0 W/m-K @Temperature 100 °C |
83.3 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
CoorsTek ADOS-90R 91% Alumina Thick Film Substrate This 91-percent alumina (nominal) formulation offers a dark brown body for special applications. Applications: thick films and lasers |
|||
Thermal Conductivity | 12.0 W/m-K @Temperature 400 °C |
83.3 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
CoorsTek ADS-96R 96% Alumina Thick Film Substrate This high-purity material ensures strong, reliable performance for ceramic substrate application. Applications: thick films and lasers |
|||
Thermal Conductivity | 12.0 W/m-K @Temperature 400 °C |
83.3 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
CoorsTek ADSR-96R DuraStrate™ 96% Alumina Thick Film Applications: thick films and lasers |
|||
Thermal Conductivity | 12.0 W/m-K @Temperature 100 °C |
83.3 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Sheet, Annealed at 2075°F (1135°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is.. |
|||
Thermal Conductivity | 12.0 W/m-K @Temperature 100 °C |
83.3 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is.. |
|||
Thermal Conductivity | 12.0 W/m-K @Temperature 100 °C |
83.3 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Bar, Annealed at 2075°F (1135°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is.. |