Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 16.0 W/m-K @Temperature 300 °C |
111 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2025°F (1107°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Thermal Conductivity | 16.0 W/m-K @Temperature 300 °C |
111 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Thermal Conductivity | 16.0 W/m-K @Temperature 400 °C |
111 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
HP Alloys Alloy B-2, Solution Treated, 20% Cold Worked Solution Treated, 20% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
Thermal Conductivity | 16.0 W/m-K @Temperature 400 °C |
111 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
HP Alloys Alloy B-2, Solution Treated, 30% Cold Worked Solution Treated, 30% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
Thermal Conductivity | 16.0 W/m-K @Temperature 400 °C |
111 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
HP Alloys Alloy B-2, Solution Treated, 40% Cold Worked Solution Treated, 40% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
Thermal Conductivity | 16.0 W/m-K @Temperature 300 °C |
111 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Special Metals INCOLOY® alloy 864 INCOLOY® alloy 8684 (UNS S35135) was specifically developed for automotive exhaust system flexible couplings, EGR tubes, manifolds and tailpipes. It exhibits excellent fatigue resistance, therma.. |
|||
Thermal Conductivity | 16.0 W/m-K @Temperature 400 °C |
111 BTU-in/hr-ft²-°F @Temperature 752 °F |
Hardened Condition |
Bohler-Uddeholm BÖHLER W302 SUPERIOR® Premium H13 Tool Steel A premium grade H13 hot work tool steel featuring:Very good toughness properties meeting the requirements of NADCA 207-97, and the superior quality levels of NADCA 207-2003Very good heat checking re.. |
|||
Thermal Conductivity | 16.0 W/m-K @Temperature 20.0 °C |
111 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
hardened to 50 HRC |
Bohler-Uddeholm UDDEHOLM STAVAX® ESR Modified 420 Premium grade stainless tool steelStavax® ESR is characterized by: Good corrosion resistance Good polishability Good wear resistance Good machinability Good stability in hardeningApplications: Udd.. |
|||
Thermal Conductivity | 16.0 W/m-K @Temperature 300 °C |
111 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Sheet, Annealed at 2075°F (1135°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is.. |
|||
Thermal Conductivity | 16.0 W/m-K @Temperature 300 °C |
111 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is.. |
|||
Thermal Conductivity | 16.0 W/m-K @Temperature 400 °C |
111 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
HP Alloys Alloy B-2, Solution Treated, 50% Cold Worked Solution Treated, 50% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |