Thermal Properties Metric English Comments
Thermal Conductivity 11.4 W/m-K

@Temperature 100 °C
79.1 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes Hastelloy® C-4 alloy, all-weld metal, as welded, GTAW
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) rang..
Thermal Conductivity 11.4 W/m-K

@Temperature 100 °C
79.1 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes Hastelloy® C-4 alloy, welded plate 12.7 mm (1/2 in.) thick, aged 1000 hours at 649°C (1200°F)
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) rang..
Thermal Conductivity 11.4 W/m-K

@Temperature 93.0 °C
79.1 BTU-in/hr-ft²-°F

@Temperature 199 °F
Annealed
Special Metals INCONEL® alloy 783 Ni-Co-Fe Alloy
The newest of the high-performance superalloys invented by Special Metals Corporation, INCONEL® alloy 783 (UNS R30783/US Patent 5,478,417), is an oxidation-resistant, low expansion, nickel-cobalt..
Thermal Conductivity 11.4 W/m-K

@Temperature 100 °C
79.1 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes Hastelloy® C-4 alloy, welded plate 12.7 mm (1/2 in.) thick, aged 10 hours at 649°C (1200°F)
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T..
Thermal Conductivity 11.4 W/m-K

@Temperature 100 °C
79.1 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes Hastelloy® C-4 alloy, welded plate 12.7 mm (1/2 in.) thick, GTAW
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T..