Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 10.0 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 10.0 W/m-K

@Temperature 25.0 °C
69.4 BTU-in/hr-ft²-°F

@Temperature 77.0 °F
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2025°F (1107°C)
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicat..
Thermal Conductivity 10.0 W/m-K

@Temperature 25.0 °C
69.4 BTU-in/hr-ft²-°F

@Temperature 77.0 °F
Haynes Hastelloy® G-35® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicat..
Thermal Conductivity 10.0 W/m-K

@Temperature 25.0 °C
69.4 BTU-in/hr-ft²-°F

@Temperature 77.0 °F
Haynes Hastelloy® G-35® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicat..
Thermal Conductivity 10.0 W/m-K

@Temperature 25.0 °C
69.4 BTU-in/hr-ft²-°F

@Temperature 77.0 °F
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2075°F (1135°C)
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicat..
Thermal Conductivity 10.0 W/m-K

@Temperature 25.0 °C
69.4 BTU-in/hr-ft²-°F

@Temperature 77.0 °F
Haynes Hastelloy® G-35® Nickel Alloy Sheet, Annealed at 2075°F (1135°C)
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is..
Thermal Conductivity 10.0 W/m-K

@Temperature 25.0 °C
69.4 BTU-in/hr-ft²-°F

@Temperature 77.0 °F
Haynes Hastelloy® G-35® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is..
Thermal Conductivity 10.0 W/m-K

@Temperature 25.0 °C
69.4 BTU-in/hr-ft²-°F

@Temperature 77.0 °F
Haynes Hastelloy® G-35® Nickel Alloy Bar, Annealed at 2075°F (1135°C)
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is..