Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.95 W/m-K @Temperature 100 °C |
13.5 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast LP 60 A Dense Refractory Brick Description: This quality combines a dense structure with a very good thermal shock resistance. The extremely low porosity results in a very good slag resistance, a good abrasion resistance and high.. |
|||
Thermal Conductivity | 1.95 W/m-K @Temperature 650 °C |
13.5 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Gouda Vuurvast LP 60 A Dense Refractory Brick Description: This quality combines a dense structure with a very good thermal shock resistance. The extremely low porosity results in a very good slag resistance, a good abrasion resistance and high.. |
|||
Thermal Conductivity | 1.95 W/m-K @Temperature 1100 °C |
13.5 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Gouda Vuurvast LP 60 A Dense Refractory Brick Description: This quality combines a dense structure with a very good thermal shock resistance. The extremely low porosity results in a very good slag resistance, a good abrasion resistance and high.. |
|||
Thermal Conductivity | 1.95 W/m-K @Temperature 100 °C |
13.5 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast AK 65 A Dense Refractory Brick Description: This andalusite based brick with a very pure mullite bond has a low alkali and iron content. In addition, it has a high creep resistance and is therefore used in applications where load.. |
|||
Thermal Conductivity | 1.95 - 2.15 W/m-K @Temperature 100 °C |
13.5 - 14.9 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast VIBRON 180 Dense Vibrating Refractory Castable Description: Vibron 180 is a low cement castable with an alumina bond. The material is supplied in two components. The B component is a liquid.Remarks: Indicated values apply to vibrated products.In.. |
|||
Thermal Conductivity | 1.95 - 2.15 W/m-K @Temperature 100 °C |
13.5 - 14.9 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast VIBRON 180 RAPID Dense Vibrating Refractory Castable Description: Vibron 180 Rapid is a low cement castable based on corundum with a special addition to enable a faster heating schedule. The material is supplied in two components. The B component cont.. |
|||
Thermal Conductivity | 1.95 - 2.15 W/m-K @Temperature 100 °C |
13.5 - 14.9 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast VIBRON 180 T Dense Vibrating Refractory Castable Description: Vibron 180 T is a low cement castable, based on tabular alumina.Remarks: Indicated values apply to vibrated products.Information provided by Gouda Vuurvast. |
|||
Thermal Conductivity | 1.95 W/m-K @Temperature 200 °C |
13.5 BTU-in/hr-ft²-°F @Temperature 392 °F |
Warp direction |
COI Ceramics Sylramic™ S200 Silicon Carbide Ceramic Matrix Composite, CG Nicalon Engineered ceramic composite structure.Reinforcing Fiber Flexibility: S400 - Carbon Preceramic Polymer Matrix Precursors: S400 - Crystalline (SiC + Si3N4) or SiCPhysical Attributes: Dense Matrix ( |
|||
Thermal Conductivity | 1.95 W/m-K @Temperature 200 °C |
13.5 BTU-in/hr-ft²-°F @Temperature 392 °F |
Fill direction |
COI Ceramics Sylramic™ S200 Silicon Carbide Ceramic Matrix Composite, CG Nicalon Engineered ceramic composite structure.Reinforcing Fiber Flexibility: S400 - Carbon Preceramic Polymer Matrix Precursors: S400 - Crystalline (SiC + Si3N4) or SiCPhysical Attributes: Dense Matrix ( |
|||
Thermal Conductivity | 1.95 W/m-K @Temperature 1000 °C |
13.5 BTU-in/hr-ft²-°F @Temperature 1830 °F |
Thru-thickness |
COI Ceramics Sylramic™ S200 Silicon Carbide Ceramic Matrix Composite, CG Nicalon Engineered ceramic composite structure.Reinforcing Fiber Flexibility: S400 - Carbon Preceramic Polymer Matrix Precursors: S400 - Crystalline (SiC + Si3N4) or SiCPhysical Attributes: Dense Matrix ( |
|||
Thermal Conductivity | 1.95 W/m-K @Temperature 700 °C |
13.5 BTU-in/hr-ft²-°F @Temperature 1290 °F |
Fill direction |
COI Ceramics Sylramic™ S200 Silicon Carbide Ceramic Matrix Composite, CG Nicalon Engineered ceramic composite structure.Reinforcing Fiber Flexibility: S400 - Carbon Preceramic Polymer Matrix Precursors: S400 - Crystalline (SiC + Si3N4) or SiCPhysical Attributes: Dense Matrix ( |
|||
Thermal Conductivity | 1.95 W/m-K @Temperature 700 °C |
13.5 BTU-in/hr-ft²-°F @Temperature 1290 °F |
Warp direction |
COI Ceramics Sylramic™ S200 Silicon Carbide Ceramic Matrix Composite, CG Nicalon Engineered ceramic composite structure.Reinforcing Fiber Flexibility: S400 - Carbon Preceramic Polymer Matrix Precursors: S400 - Crystalline (SiC + Si3N4) or SiCPhysical Attributes: Dense Matrix ( |
|||
Thermal Conductivity | 1.95 W/m-K @Temperature 1100 °C |
13.5 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Gouda Vuurvast LP 60 M Dense Refractory Brick Description: LP 60 M is a special low porosity, high strength material based on raw materials with a high mullite content. The grain distribution for these bricks is carefully selected, so that a ma.. |