Thermal Properties Metric English Comments
Thermal Conductivity 0.2792 W/m-K

@Temperature 800 °C
1.934 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Chosun Refractories GUN-100L Light-Weight Gunning Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Thermal Conductivity 0.2792 W/m-K

@Temperature 260 °C
1.934 BTU-in/hr-ft²-°F

@Temperature 500 °F
Chosun Refractories GUN-110L Light-Weight Gunning Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Thermal Conductivity 0.2792 W/m-K

@Temperature 540 °C
1.934 BTU-in/hr-ft²-°F

@Temperature 1000 °F
Chosun Refractories INCT-120S Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).