Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.93 W/m-K @Temperature 650 °C |
13.4 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Gouda Vuurvast AK 65 A Dense Refractory Brick Description: This andalusite based brick with a very pure mullite bond has a low alkali and iron content. In addition, it has a high creep resistance and is therefore used in applications where load.. |
|||
Thermal Conductivity | 1.93 W/m-K @Temperature 1100 °C |
13.4 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Gouda Vuurvast AK 65 A Dense Refractory Brick Description: This andalusite based brick with a very pure mullite bond has a low alkali and iron content. In addition, it has a high creep resistance and is therefore used in applications where load.. |
|||
Thermal Conductivity | 1.93 - 2.13 W/m-K @Temperature 600 °C |
13.4 - 14.8 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast VIBRON 180 Dense Vibrating Refractory Castable Description: Vibron 180 is a low cement castable with an alumina bond. The material is supplied in two components. The B component is a liquid.Remarks: Indicated values apply to vibrated products.In.. |
|||
Thermal Conductivity | 1.93 - 2.13 W/m-K @Temperature 600 °C |
13.4 - 14.8 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast VIBRON 180 RAPID Dense Vibrating Refractory Castable Description: Vibron 180 Rapid is a low cement castable based on corundum with a special addition to enable a faster heating schedule. The material is supplied in two components. The B component cont.. |
|||
Thermal Conductivity | 1.93 - 2.13 W/m-K @Temperature 600 °C |
13.4 - 14.8 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast VIBRON 180 T Dense Vibrating Refractory Castable Description: Vibron 180 T is a low cement castable, based on tabular alumina.Remarks: Indicated values apply to vibrated products.Information provided by Gouda Vuurvast. |