Thermal Properties Metric English Comments
Thermal Conductivity 1.31 - 1.51 W/m-K

@Temperature 100 °C
9.09 - 10.5 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURAS 90 D Moldable Refractory Material
Description: This material is supplied as a dry powder, it has to be mixed with potable water to the necessary consistency. This high refractory ramming material contains several well defined corund..