Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.22 - 1.32 W/m-K @Temperature 1000 °C |
8.47 - 9.16 BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
Gouda Vuurvast CURON 120 S Dense Refractory Castable Description: A very strong castable with a high abrasion resistance of which both aggregate and cement attribute to hydraulic binding.Remarks: These values apply to cast products. Also available in .. |