Thermal Conductivity 0.163 W/m-K

@Temperature 150 °C
1.13 BTU-in/hr-ft²-°F

@Temperature 302 °F
ASTM D1674
DuPont™ Nomex® Type 994, 125 mil Nominal Thickness Rigid Aromatic Nylon Board
Type 994 is a densified, rigid board which has a unique combination of superior resistance to compression, even at elevated temperatures, along with relatively high oil absorption characteristics. T..