Thermal Conductivity 1.04 - 1.24 W/m-K

@Temperature 1100 °C
7.22 - 8.61 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Gouda Vuurvast CURAS 40 Moldable Refractory Material
Description: Because of special additions this type of moldable already has a reasonable strength at room temperature. It is used for a wide range of applications.Remarks: The stated chemical compos..