Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.0236 W/m-K @Temperature 500 °C |
7.0921 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Chosun Refractories PT-170 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Thermal Conductivity | 1.0236 W/m-K @Temperature 1000 °C |
7.0921 BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
Chosun Refractories PAC-160 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |