Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.890 - 0.990 W/m-K @Temperature 100 °C |
6.18 - 6.87 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURAS 85 P Moldable Refractory Material Description: This phosphate bonded material based on corundum and bauxite has already at low temperature a reasonable strength and has a very good resistance against slag attack or liquid aluminum. .. |
|||
Thermal Conductivity | 0.890 - 0.990 W/m-K @Temperature 100 °C |
6.18 - 6.87 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURAS 85 PD Moldable Refractory Material Description: This material is supplied as a dry powder, it has to be mixed with potable water to the necessary consistency. This phosphate bonded material based on corundum and bauxite has a very go.. |
|||
Thermal Conductivity | 0.890 - 0.990 W/m-K @Temperature 100 °C |
6.18 - 6.87 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURAS 85 PD GM Moldable Refractory Material Description: This material is supplied as a dry powder and can be gunned. This phosphate bonded material based on corundum and bauxite has a very good resistance against slag attack or liquid alumin.. |