Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.125 W/m-K @Temperature 400 °C |
0.868 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Pyrotek Pyrite N-14 Refractory Board Pyrotek N-14 is a fiberglass reinforced calcium silicate board specifically developed for the non-ferrous industry. The superior strength and unique formulation of Pyrotek N-14 makes it the preferr.. |
|||
Thermal Conductivity | 0.125 W/m-K @Temperature 200 °C |
0.868 BTU-in/hr-ft²-°F @Temperature 392 °F |
Mean temp.; ASTMÂ C-182 |
Skamol Group Moler SM-65 Insulating Block SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str.. |