Polymer Property : Thermal Conductivity = 0.861 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.124 W/m-K

@Temperature 300 °C
0.861 BTU-in/hr-ft²-°F

@Temperature 572 °F
Pyrotek Pyrite N-17 Refractory Board
Pyrotek N-17 is a graphite fiber reinforced, high purity, calcium silicate board developed exclusively for the non-ferrous casting industry. The patented formulation of Pyrotek N-17 makes it good i..