Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.123 W/m-K @Temperature 100 °C |
0.854 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Pyrotek Pyrite N-14 Refractory Board Pyrotek N-14 is a fiberglass reinforced calcium silicate board specifically developed for the non-ferrous industry. The superior strength and unique formulation of Pyrotek N-14 makes it the preferr.. |