Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.116 - 0.174 W/m-K @Temperature 540 °C |
0.806 - 1.21 BTU-in/hr-ft²-°F @Temperature 1000 °F |
|
Chosun Refractories MIX-3 Light-Weight Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Thermal Conductivity | 0.116 - 0.174 W/m-K @Temperature 800 °C |
0.806 - 1.21 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Chosun Refractories MIX-3 Light-Weight Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |