Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.112 W/m-K @Temperature 149 °C |
0.780 BTU-in/hr-ft²-°F @Temperature 300 °F |
|
Paratherm Corporation Paratherm™ GLT™ Heat Transfer Fluid Paratherm GLT™ Heat Transfer Fluid is an alkylated aromatic based heat transfer fluid formulated for closed loop liquid phase heating systems to 550°F using fired heaters and to 575°F in waste-he.. |