Polymer Property : Thermal Conductivity = 0.750 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.750 - 0.850 W/m-K

@Temperature 100 °C
5.20 - 5.90 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURON 160 Dense Refractory Castable
Description: Because of the selection of raw materials this castable has a high volume stability and maintains its strength up to high temperatures. In addition Curon 160 has an excellent thermal sh..
Thermal Conductivity 0.750 W/m-K

@Temperature 1000 °C
5.20 BTU-in/hr-ft²-°F

@Temperature 1830 °F
parallel to thickness; ASTM C1113
Zircar Refractory Composites RSLE-501 CYLINDERS Refractory Sheet
ZIRCAR Refractory Sheet Type RSLE-501 is a low expansion high strength reinforced silica matrix composites in a cylindrical form. This material was designed for use as a high strength, durable insul..
Thermal Conductivity 0.750 W/m-K

@Temperature 1000 °C
5.20 BTU-in/hr-ft²-°F

@Temperature 1830 °F
parallel to thickness; ASTM C1113
Zircar Refractory Composites RSLE-56 MOLDABLE Refractory Sheet
ZIRCAR Refractory Sheet Type RSLE-56 Moldable is a high silica fiber reinforced ceramic composite material that is easily cut and formed into flat sheets in addition to a wide variety of simple and ..
Thermal Conductivity 0.750 W/m-K

@Temperature 1000 °C
5.20 BTU-in/hr-ft²-°F

@Temperature 1830 °F
parallel to thickness; ASTM C1113
Zircar Refractory Composites RSLE-57 Refractory Sheet
ZIRCAR Refractory Sheet Type RSLE-57 is a low expansion high strength reinforced silica matrix composite . This material was designed for use as a high strength insulator in induction hot press appl..