Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.720 - 0.820 W/m-K @Temperature 600 °C |
5.00 - 5.69 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 150 GM Dense Refractory Castable Description: Curon 150 GM is a gunmix based on sintered bauxite with an excellent thermal shock resistance and is therefore very well suited for burner blocks.Remarks: These values apply to cast pro.. |