Polymer Property : Thermal Conductivity = 0.700 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.700 - 0.800 W/m-K

@Temperature 100 °C
4.86 - 5.55 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURAS 50 PD Moldable Refractory Material
Description: This material is supplied as a dry powder, it has to be mixed with potable water to the necessary consistency. Because of the addition of phosphate this type of moldable has a high stre..
Thermal Conductivity 0.700 - 0.900 W/m-K

@Temperature 100 °C
4.86 - 6.25 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURON 180 L Dense Refractory Castable
Description: Curon 180 L is a castable based on fused alumina for use up to 1800°C and shows a good thermal shock resistance.Remarks: These values apply to cast products. Also available in gunnin..
Thermal Conductivity 0.700 - 0.800 W/m-K

@Temperature 100 °C
4.86 - 5.55 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURAS 40 D Moldable Refractory Material
Description: This material is supplied as a dry powder, it has to be mixed with potable water to the necessary consistency. Because of special additions this type of moldable has already a reasonabl..
Thermal Conductivity 0.700 - 0.800 W/m-K

@Temperature 100 °C
4.86 - 5.55 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURAS 40 PD Moldable Refractory Material
Description: This material is supplied as a dry powder, it has to be mixed with potable water to the necessary consistency. Because of the addition of phosphate this type of moldable has a high stre..
Thermal Conductivity 0.700 - 0.800 W/m-K

@Temperature 100 °C
4.86 - 5.55 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURAS 50 D Moldable Refractory Material
Description: Because of special additions this moldable already has a reasonable strength at room temperature. This material is supplied as a dry powder, it has to be mixed with potable water to the..
Thermal Conductivity 0.700 - 0.800 W/m-K

@Temperature 600 °C
4.86 - 5.55 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURON 165 GM Dense Refractory Castable
Description: Curon 165 GM is based on bauxite and very pure chamotte grog. In has very good thermal shock resistance and a low firing shrinkage.Remarks: These values apply to cast products. Other mo..
Thermal Conductivity 0.700 W/m-K

@Temperature 500 °C
4.86 BTU-in/hr-ft²-°F

@Temperature 932 °F
Touchstone CFOAM® 20 Structural Carbon Foam
CFOAM, developed by Touchstone Research Laboratory, Ltd., is a next generation structural material which is inexpensive, lightweight, fire-resistant, impact-absorbing, and which can be thermally ins..