Polymer Property : Thermal Conductivity = 0.590 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.0850 W/m-K

@Temperature 149 °C
0.590 BTU-in/hr-ft²-°F

@Temperature 300 °F
x-ply; 8HS form; ASTM C177
Park Electrochemical Nelcote® F-555 Phenolic Prepreg, NARC/CYDSA Reinforced
Nelcote® F-555 is a carbon-filled MIL-R-9299 phenolic resin optimized for coating Carbonized Rayon cloth. F-555 is used extensively in the manufacture of high temperature rocket nozzles, heat shiel..
Thermal Conductivity 0.0850 W/m-K

@Temperature 400 °C
0.590 BTU-in/hr-ft²-°F

@Temperature 752 °F
@ 110 kg/m³; ASTM C177, ISO 8302, DIN EN-12667:2001-05
Microtherm Group MT Thermosphere® Moldable Insulation Paste
MT Thermosphere® is a low density temperature resistant paste with excellent thermal insulation properties from cryogenic to high temperature exposure. It is a perfectly seamless insulation syste..